Plastic Flexible PA Air Tube (12*8mm)

  • Price:

    Negotiable

  • minimum:

  • Total supply:

  • Delivery term:

    The date of payment from buyers deliver within days

  • seat:

    Shanghai

  • Validity to:

    Long-term effective

  • Last update:

    2017-12-22 06:01

  • Browse the number:

    74

Send an inquiries

Company Profile

Shanghai Zhengmi Pneumatic Element Co., Ltd.

By certification [File Integrity]

Contact:Miss Sammi(Mr.)  

Email:

Telephone:

Area:Shanghai

Address:Shanghai

Website: http://zhengmipneumatic.jshongxingchem.com/

Product details


PA11,12 Nylon tube function:
Good wear ability,smooth surface,low resistance,anti-rustiness and an ti-scaling.
Flexible,easily to be bended into all kinds of shapes,easy to install.
High chemical and hydrolysis resistance,stable dimension,little penetration,can be used long time.
High and low temperature resistance(-40~100°),can transfer compressed air,water,oil chemical liquid and so on.
 
PA11,12 tube used area:
Light trucks,car hydraulic brake system.
power steering tube.
mechanical transmission and control system piping.
paint and liquid resin spraying high-pressure pipe.
air conditioning.



PA Tube Size :
note:the following size is just for you refer , unstandard size is custom-made .
ITEM NO. ID*OD WORKING PRESSURE MAX PRESSURE BEVELLING RADIUS
PA0420 4*2mm 45bar 135bar 30mm
PA0530 5*3mm 34bar 102bar 35mm
PA0640 6*4mm 27m 81bar 40mm
PA0860 8*6mm 19mm 57bar 50mm
PA1075 10*7.5mm 15mm 45bar 60mm
PA1080 10*8mm 15mm 45bar 65mm
PA1290 12*9mm 19mm 57bar 70mm
PA1410 14*10mm 19mm 57bar 100mm
PA1612 16*12mm 19mm 57bar 130mm

 
Notice:
1. Tubes are with the risk of burst if they work under such conditions: high temperature (>60°C), corrosive fluid (strong acid, alkali, or solvent).
2. High temperature (>60°C) cause softens of tube and the limitation of burst pressure would be reduced. Also chemical gas in air might speed up the aging and cracking of tube.
3. Please do not put tubes under humid environment or store them for a long period (>180 days), otherwise, it becomes cracking due to hydrolysis effect.